Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.17 - 1.64 g/cc
0.0423 - 0.0592 lb/in³
Average value: 1.41 g/cc Grade Count:48
Water Absorption 0.0600 - 0.400 %
0.0600 - 0.400 %
Average value: 0.155 % Grade Count:14
Moisture Absorption at Equilibrium 0.0800 - 0.160 %
0.0800 - 0.160 %
Average value: 0.120 % Grade Count:15
Water Absorption at Saturation 0.100 - 0.500 %
0.100 - 0.500 %
Average value: 0.349 % Grade Count:10
Maximum Moisture Content 0.0200
0.0200
Average value: 0.0200 Grade Count:3
Linear Mold Shrinkage 0.000500 - 0.0100 cm/cm
0.000500 - 0.0100 in/in
Average value: 0.00488 cm/cm Grade Count:39
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00605 cm/cm Grade Count:16
Melt Flow 3.20 - 56.0 g/10 min
3.20 - 56.0 g/10 min
Average value: 25.3 g/10 min Grade Count:24
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95.0 - 119
95.0 - 119
Average value: 115 Grade Count:15
Hardness, H358/30 95.0 - 115 MPa
13800 - 16700 psi
Average value: 104 MPa Grade Count:4
Tensile Strength, Ultimate 45.0 - 138 MPa
6530 - 20000 psi
Average value: 93.7 MPa Grade Count:35
Tensile Strength, Yield 48.0 - 114 MPa
6960 - 16500 psi
Average value: 88.2 MPa Grade Count:22
Elongation at Break 1.00 - 200 %
1.00 - 200 %
Average value: 11.2 % Grade Count:40
Elongation at Yield 1.00 - 3.60 %
1.00 - 3.60 %
Average value: 2.29 % Grade Count:9
Modulus of Elasticity 2.80 - 13.8 GPa
406 - 2000 ksi
Average value: 7.28 GPa Grade Count:22
Flexural Yield Strength 85.0 - 207 MPa
12300 - 30000 psi
Average value: 151 MPa Grade Count:37
Flexural Modulus 1.72 - 13.1 GPa
250 - 1900 ksi
Average value: 5.78 GPa Grade Count:42
Izod Impact, Notched 0.427 - 10.8 J/cm
0.800 - 20.2 ft-lb/in
Average value: 1.68 J/cm Grade Count:32
0.600 - 1.12 J/cm

@Temperature -30.0 - -30.0 °C
1.12 - 2.10 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.864 J/cm Grade Count:9
1.01 - 1.07 J/cm

@Temperature -20.0 - -20.0 °C
1.89 - 2.00 ft-lb/in

@Temperature -4.00 - -4.00 °F
Average value: 0.864 J/cm Grade Count:2
1.01 - 1.07 J/cm

@Thickness 3.18 - 3.18 mm
1.89 - 2.00 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.864 J/cm Grade Count:2
Izod Impact, Unnotched 5.93 - 9.50 J/cm
11.1 - 17.8 ft-lb/in
Average value: 6.63 J/cm Grade Count:13
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²
1.43 - 4.76 ft-lb/in²
Average value: 6.86 kJ/m² Grade Count:14
3.00 - 11.0 kJ/m²

@Temperature -30.0 - 0.000 °C
1.43 - 5.23 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 5.71 kJ/m² Grade Count:13
Izod Impact, Unnotched (ISO) 25.0 - 55.0 kJ/m²
11.9 - 26.2 ft-lb/in²
Average value: 40.2 kJ/m² Grade Count:6
27.0 - 80.0 kJ/m²

@Temperature -30.0 - -30.0 °C
12.8 - 38.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 46.8 kJ/m² Grade Count:5
Charpy Impact Unnotched 2.70 - 5.50 J/cm²
12.8 - 26.2 ft-lb/in²
Average value: 4.17 J/cm² Grade Count:10
2.20 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
10.5 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.64 J/cm² Grade Count:5
Charpy Impact, Notched 0.400 - 2.10 J/cm²
1.90 - 9.99 ft-lb/in²
Average value: 1.28 J/cm² Grade Count:12
0.300 - 1.00 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.675 J/cm² Grade Count:4
Dart Drop, Total Energy 5.00 - 17.0 J
3.69 - 12.5 ft-lb
Average value: 8.27 J Grade Count:10
3.00 - 7.00 J

@Temperature -30.0 - -20.0 °C
2.21 - 5.16 ft-lb

@Temperature -22.0 - -4.00 °F
Average value: 3.75 J Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 21.0 - 450 µm/m-°C
11.7 - 250 µin/in-°F
Average value: 57.6 µm/m-°C Grade Count:24
16.2 - 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
9.00 - 12.0 µin/in-°F

@Temperature 140 - 280 °F
Average value: 18.6 µm/m-°C Grade Count:6
CTE, linear, Transverse to Flow 30.0 - 110 µm/m-°C
16.7 - 61.1 µin/in-°F
Average value: 78.9 µm/m-°C Grade Count:15
Thermal Conductivity 0.180 - 0.190 W/m-K
1.25 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.187 W/m-K Grade Count:3
Melting Point 220 - 225 °C
428 - 437 °F
Average value: 224 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 108 - 215 °C
226 - 419 °F
Average value: 170 °C Grade Count:31
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 195 °C
145 - 383 °F
Average value: 138 °C Grade Count:47
Vicat Softening Point 121 - 212 °C
250 - 414 °F
Average value: 154 °C Grade Count:16
UL RTI, Electrical 75.0 - 140 °C
167 - 284 °F
Average value: 117 °C Grade Count:9
UL RTI, Mechanical with Impact 75.0 - 130 °C
167 - 266 °F
Average value: 107 °C Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 5.90e+16 ohm-cm
1.00e+14 - 5.90e+16 ohm-cm
Average value: 2.23e+16 ohm-cm Grade Count:13
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Average value: 1.00e+15 ohm Grade Count:6
Dielectric Constant 2.90 - 4.00
2.90 - 4.00
Average value: 3.53 Grade Count:15
Dielectric Strength 14.0 - 34.0 kV/mm
356 - 864 kV/in
Average value: 23.3 kV/mm Grade Count:14
Dissipation Factor 0.00100 - 0.0200
0.00100 - 0.0200
Average value: 0.00988 Grade Count:12
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 105 sec Grade Count:8
Comparative Tracking Index 100 - 400 V
100 - 400 V
Average value: 184 V Grade Count:11
Hot Wire Ignition, HWI 60.0 - 120 sec
60.0 - 120 sec
Average value: 90.0 sec Grade Count:6
High Amp Arc Ignition, HAI 15.0 - 30.0 arcs
15.0 - 30.0 arcs
Average value: 22.5 arcs Grade Count:6
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 67.6 mm/min Grade Count:6
Users viewing this material also viewed the following: