Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 - 215 °C
226 - 419 °F
Average value: 170 °C Grade Count:31
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
Average value: 213 °C Grade Count:3
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 215 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 220 01HB Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 220 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 220 12V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 230 01HB Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 230 12V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 220 12HB Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Loxim 230 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 105 - 215 °C
221 - 419 °F
Average value: 166 °C Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Deflection Temperature at 0.46 MPa (66 psi) 110 - 215 °C
230 - 419 °F
Average value: 176 °C Grade Count:30
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Deflection Temperature at 0.46 MPa (66 psi) 143 - 215 °C
290 - 419 °F
Average value: 166 °C Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..