Material Notes:
Product description: Grilon BM 16 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 16 natural has the following features: High flexibility and toughnessVery good orientation and thermoforming propertiesHigh shrinkageVery good transparencyLow melting point (164°C)Low glass transition point (44°C) Application Examples: Grilon BM 16 natural has been specially developed for cast and blown films coextruded with temperature sensitive polymers (PVDC, EVOH). Grilon BM 16 natural is suitable flexible packaging for foodstuffs e.g. (shrinkable) film for consumer packaging of meat, cheese, sausage or fish.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 10 %
10 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 16.0 g/m²/day
1.03 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 70.0 cc/m²/day
4.51 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
90.0 cc/m²/day
5.80 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 200 cc-mm/m²-24hr-atm
508 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
300 cc-mm/m²-24hr-atm
762 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 100 g/10 min
100 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 0.500 GPa
72.5 ksi
conditioned; ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 164 °C
327 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 64 %
64 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
Form Granules
Packaging Non oriented film
Oriented film
Paper coating
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
High viscosity
Transparent Polyamide
Special Characteristics Transparent