Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 195 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 195 °C
145 - 383 °F
Average value: 138 °C Grade Count:47
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..