Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 °C |
9.00 µin/in-°F @Temperature 68.0 °F |
|
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
CTE, linear | 16.2 - 46.8 µm/m-°C | 9.00 - 26.0 µin/in-°F | Average value: 34.0 µm/m-°C Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 21.1 - 102 °C |
9.00 µin/in-°F @Temperature 70.0 - 215 °F |
|
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 95.0 °C |
9.00 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 2 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 25.0 - 500 °C |
9.00 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Porta Maximum PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 715 Copper Nickel 30%, Annealed 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 715 Copper Nickel 30%, Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 735 Nickel Silver 18%, 1/4 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 735 Nickel Silver 18%, Extra Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 735 Nickel Silver 18%, Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 735 Nickel Silver 18%, Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 752 Nickel Silver 18%, Annealed Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 752 Nickel Silver 18%, Extra Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 762 Nickel Silver 12%, Extra Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Carlson 70 30 Cu Ni Copper-Nickel Alloy General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp.. |
|||
CTE, linear | 16.2 - 20.0 µm/m-°C | 9.00 - 11.1 µin/in-°F | Average value: 18.3 µm/m-°C Grade Count:7 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 300 °C |
9.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 752 Nickel Silver 18%, Extra Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
CTE, linear | 16.2 - 27.0 µm/m-°C | 9.00 - 15.0 µin/in-°F | Average value: 21.9 µm/m-°C Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 16.2 µm/m-°C @Temperature 20.0 - 95.0 °C |
9.00 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
CTE, linear | 16.2 - 130 µm/m-°C | 9.00 - 72.2 µin/in-°F | Average value: 35.9 µm/m-°C Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |