Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Nylene® CX3451 Translucent Nylon Copolymer Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Nylene® Naxel™ B720 Polycarbonate/PBT Alloy Description: Naxel™ B720 is a Polycarbonate/PBT alloy. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Flamâ„¢ 205 HFRI Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | tangent; ASTM D790 |
Spartech PP5210 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR-N IM Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: .. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company PermaStat® 800 Acetal (POM), Permanently Anti-static - ESD Protection |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company RTP 100 MS 2 Polypropylene (PP), Molybdenum Disulfide - Preliminary Data |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company RTP 101 HI Z Polypropylene (PP) Glass Fiber - Impact Modified - FDA Compliant Ingredients |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company RTP 200 F AR 10 TFE 10 Nylon 12 (PA) Aramid Fiber - PTFE Lubricated - Preliminary Data |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company PermaStat® 1800 MD Acrylic (PMMA); Permanently Anti-static - ESD Protection - Transparent Grade |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company RTP 200 H TFE 20 SI 1 Impact-Modified Nylon 6/6 (PA), PTFE Lubricated - Silicone Lubricated |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Chesterton MRS S4+ Metal Rebuilding System An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 .. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Asahi Kasei Thermofil P-9900-0712 Unfilled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH200LN-02 Polypropylene, Homopolymer, Rx grade, Nucleated, Lube, Injection Molding COPYLENE™ CH200LN-02 is a polypropylene homopolymer resin nucleated for faster crystallization with antistatic properties and designed for injection molding applications. Applications: Caps & Closu.. |
|||
Flexural Modulus | 1.72 - 3.45 GPa | 250 - 500 ksi | Average value: 2.69 GPa Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
RTP Company RTP 3200 MG 20 Ethylene Tetrafluoroethylene (ETFE), Milled Glass |