Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 263R PC (Europe-Africa-Middle East) LEXAN 263R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 923 PC (Europe-Africa-Middle East) LEXAN 923 is a low viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 945AU PC (Europe-Africa-Middle East) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXD123R PC (Europe-Africa-Middle East) LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXD141 PC (Europe-Africa-Middle East) LEXAN FXD141 is a transparent/translucent medium viscosity grade for light diffusion effects. The color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXD143R PC (Europe-Africa-Middle East) LEXAN FXD143R is a transparent/translucent medium viscosity grade for light diffusion effects. UV-stabilized. The color package may affect performance. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXE921A PC (Europe-Africa-Middle East) LEXAN FXE921A is a transparent/translucent, medium viscosity, flame retardant grade with a fluorescent appearance. Color package may affect performance.This data was supplied by SABIC-IP for the Eur.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXG921A PC (Europe-Africa-Middle East) LEXAN FXG921A is a transparent/translucent, medium viscosity, flame retardant grade with a diamond sparkle appearance. Color package may affect performance.This data was supplied by SABIC-IP for the.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXM121R PC (Europe-Africa-Middle East) LEXAN FXM121R is a transparent/translucent low viscosity grade for special effects colors with a metallic-luster appearance. Color package may affect performance. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® HP1 PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® LI1813R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose PC having low levels of ionics species. UV-stabilized. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® OQ3120 PC (Europe-Africa-Middle East) High Flow. UV-stabilized. Inherent mold release. Ophthalmic lenses. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 925 PC (Europe-Africa-Middle East) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East) LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXD144R PC (Europe-Africa-Middle East) LEXAN FXD144R is a transparent/translucent medium viscosity grade for light diffusion effects. FDA compliant. Internal mold release. The color package may affect performance.This data was supplie.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® FXM161R PC (Europe-Africa-Middle East) LEXAN FXM161R is a transparent/translucent medium viscosity grade for special effects colours with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East) XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | DAM; DS; ISO 2039-1 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |