Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Optrene 10GF Polypropylene Chemically coupled glass reinforced(10%) polypropylene with high strength and HDT.Information provided by Ovation Polymers |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min |
Polimeri Europa KOBLEND HI PD 41 G1 PBT+PC, 5% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1: PBT+PC (GF) Elastomer modified PBT+PC blend reinforced with 5% of glass fibres, a good combination of stiffness, dimensional stability and thoughness. Main applicat.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | |
Ineos ABS LUSTROPAK® 1010 ABS, Extrusion Grade
(discontinued **) Extrusion grade, high stiffness.Applications: Food containers.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 377 Plating, Injection Molding Grade |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Tensile Strength, Yield | 48.0 MPa @Temperature 23.0 °C |
6960 psi @Temperature 73.4 °F |
50-mm/min; ISO 527 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® 357U PBT Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Strength, Yield | 48.0 MPa @Thickness 6.35 mm |
6960 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ASTM D638 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | |
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingSheet extrusionInformation provided by Bayer Polymers.As of 1 .. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 400H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ISO 527B |
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti.. |
|||
Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |