Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 79.2 - 110 µm/m-°C | 44.0 - 61.1 µin/in-°F | Average value: 89.6 µm/m-°C Grade Count:9 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
CTE, linear, Transverse to Flow | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | Average value: 89.3 µm/m-°C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
CTE, linear, Transverse to Flow | 30.0 - 110 µm/m-°C | 16.7 - 61.1 µin/in-°F | Average value: 78.9 µm/m-°C Grade Count:15 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
CTE, linear, Transverse to Flow | 92.0 - 110 µm/m-°C @Temperature 100 - 200 °C |
51.1 - 61.1 µin/in-°F @Temperature 212 - 392 °F |
Average value: 101 µm/m-°C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
CTE, linear, Transverse to Flow | 75.0 - 110 µm/m-°C | 41.7 - 61.1 µin/in-°F | Average value: 91.7 µm/m-°C Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
CTE, linear, Transverse to Flow | 10.0 - 110 µm/m-°C | 5.56 - 61.1 µin/in-°F | Average value: 66.2 µm/m-°C Grade Count:21 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
CTE, linear, Transverse to Flow | 84.0 - 110 µm/m-°C @Temperature 23.0 °C |
46.7 - 61.1 µin/in-°F @Temperature 73.4 °F |
|
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear, Transverse to Flow | 36.0 - 110 µm/m-°C | 20.0 - 61.1 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:3 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear, Transverse to Flow | 34.0 - 110 µm/m-°C | 18.9 - 61.1 µin/in-°F | Average value: 62.4 µm/m-°C Grade Count:3 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |