Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Izod Impact, Notched | >= 1.01 J/cm | >= 1.89 ft-lb/in | ASTM D256 |
NIZHNEKAMSKNEFTEKHIM 825EF High Impact Polystyrene Grade 825EF is a high impact polystyrene designed for extrusion and hot molding application. It is suited for hot molded deep drawn industrial packages and multilayer shaped sheet production via ex.. |
|||
Izod Impact, Notched | 1.01 J/cm @Temperature 23.0 °C |
1.89 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Colorcomp DX98735 PC LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | 1/8" (3mm) notched bar; ASTM D256 |
Ineos N12N-00 Polypropylene Impact Copolymer Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | |
MTI ThermoStran® PP-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized... |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66 LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® HIPS TL10 BK Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm |
1.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® EG106 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Diamond Polymers ABS TX-541 Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | injection molded; ASTM D256 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.89 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 630-33GU Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin, utility grade. Also available: 630S - 33GU Heat Stabilized, 630 - 33GBU Black, 630S - 33GBU Black with H.S.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | |
Atom Adhesives AA-BOND 201 Epoxy Adhesive AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system.. |
|||
Izod Impact, Notched | 1.01 J/cm | 1.90 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |