Thermal Properties Metric English Comments
Thermal Conductivity 0.180 - 0.190 W/m-K
1.25 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.187 W/m-K Grade Count:3
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Thermal Conductivity 0.140 - 0.190 W/m-K
0.972 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.162 W/m-K Grade Count:4
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Thermal Conductivity 0.190 - 0.190 W/m-K

@Temperature 40.0 - 40.0 °C
1.32 - 1.32 BTU-in/hr-ft²-°F

@Temperature 104 - 104 °F
Average value: 0.190 W/m-K Grade Count:1
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM C177
Zeus PVDF Tubing
PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Thermal Conductivity 0.130 - 0.190 W/m-K
0.900 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.160 W/m-K Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Thermal Conductivity 0.170 - 0.190 W/m-K

@Temperature 50.0 - 200 °C
1.18 - 1.32 BTU-in/hr-ft²-°F

@Temperature 122 - 392 °F
Average value: 0.180 W/m-K Grade Count:4
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved