Suzhou Hipro Polymers Hiprolon® 211 ESNNHL P40 Nylon

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer Suzhou Hipro Polymers
Trade Name Hiprolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hiprolon® 211 ESNNHL P40 Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hiprolon® 211ESNNHL P40 is a long chain polyamide compound from bio-renewable resource. It features low density, low water absorption, high dimension stability, high cold impact resistance, high burst pressure, low gasoline permeation, good chemical resistance. It is widely used for auto fuel lines, air brake tubing, cable sheathing et al and meets ISO 7628, DIN 73378, DIN 74324 standards in automotive industry.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
dry; ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
D 638
Elongation at Break 360 %
360 %
ASTM D638
Flexural Modulus 0.320 GPa
46.4 ksi
ASTM D790
Charpy Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
50% RH; DSC
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 210 - 270 °C
410 - 518 °F
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Dry Time 4 hour
4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Users viewing this material also viewed the following: