Polymer Property : Dart Drop, Total Energy = 7.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 1.00 - 7.00 J
0.738 - 5.16 ft-lb
Average value: 4.50 J Grade Count:8
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Dart Drop, Total Energy 3.00 - 7.00 J

@Temperature -30.0 - -20.0 °C
2.21 - 5.16 ft-lb

@Temperature -22.0 - -4.00 °F
Average value: 3.75 J Grade Count:3
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..