Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 - 5.50 J/cm²
9.52 - 26.2 ft-lb/in²
Average value: 3.82 J/cm² Grade Count:14
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact Unnotched 2.60 - 5.50 J/cm²
12.4 - 26.2 ft-lb/in²
Average value: 3.77 J/cm² Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Charpy Impact Unnotched 1.50 - 5.50 J/cm²
7.14 - 26.2 ft-lb/in²
Average value: 3.75 J/cm² Grade Count:4
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 5.50 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
26.2 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.50 J/cm² Grade Count:1
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 2.50 - 5.50 J/cm²
11.9 - 26.2 ft-lb/in²
Average value: 4.17 J/cm² Grade Count:3
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Charpy Impact Unnotched 2.70 - 5.50 J/cm²
12.8 - 26.2 ft-lb/in²
Average value: 4.17 J/cm² Grade Count:10
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Charpy Impact Unnotched 2.20 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
10.5 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.64 J/cm² Grade Count:5
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Charpy Impact Unnotched 1.30 - 5.50 J/cm²
6.19 - 26.2 ft-lb/in²
Average value: 3.10 J/cm² Grade Count:19
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Charpy Impact Unnotched 2.00 - 5.50 J/cm²

@Temperature -30.0 - -20.0 °C
9.52 - 26.2 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.12 J/cm² Grade Count:18
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 3.00 - 5.50 J/cm²
14.3 - 26.2 ft-lb/in²
Average value: 4.40 J/cm² Grade Count:8
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Charpy Impact Unnotched 2.00 - 5.50 J/cm²
9.52 - 26.2 ft-lb/in²
Average value: 3.92 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..