Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Voltage Arc-Tracking Rate, HVTR = 150 mm/min Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 923ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 943ASR PC (Asia Pacific)
More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 955AU PC
Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC 3
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Color package may affect performance.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC 3
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release
Information provided by Polymer Technology and Services, LLC (PTS).
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC code 3; UL 746A
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
Average value: 127 mm/min Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 940A PC
Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific)
Opaque colors, high viscosity, superior flame retardance. UV-stabilized.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC 3
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC 3
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 102 mm/min Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
Average value: 115 mm/min Grade Count:8
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min

@Thickness 3.00 mm
3.15 - 5.91 in/min

@Thickness 0.118 in
BK, BN
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, ..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics NORYL HS2000X PPE+PS
PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 940 PC
Opaque colors, medium viscosity, superior flame retardance.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 953A PC
Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Copyright © lookpolymers.com All Rights Reserved