Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse -0.00300 - 0.00900 cm/cm
-0.00300 - 0.00900 in/in
Average value: 0.00457 cm/cm Grade Count:22
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse -0.00200 - 0.00900 cm/cm
-0.00200 - 0.00900 in/in
Average value: 0.00513 cm/cm Grade Count:12
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Linear Mold Shrinkage, Transverse 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00673 cm/cm Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Linear Mold Shrinkage, Transverse 0.00750 - 0.00900 cm/cm
0.00750 - 0.00900 in/in
Average value: 0.00806 cm/cm Grade Count:8
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage, Transverse 0.00800 - 0.00900 cm/cm
0.00800 - 0.00900 in/in
Average value: 0.00867 cm/cm Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00550 cm/cm Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00605 cm/cm Grade Count:16
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00557 cm/cm Grade Count:7
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00546 cm/cm Grade Count:35
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Linear Mold Shrinkage, Transverse 0.00800 - 0.00900 cm/cm
0.00800 - 0.00900 in/in
Average value: 0.00833 cm/cm Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00654 cm/cm Grade Count:13
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00544 cm/cm Grade Count:11
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00580 cm/cm Grade Count:26
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Linear Mold Shrinkage, Transverse 0.00600 - 0.00900 cm/cm
0.00600 - 0.00900 in/in
Average value: 0.00817 cm/cm Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00599 cm/cm Grade Count:4
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00541 cm/cm Grade Count:22
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage, Transverse 0.00900 - 0.00900 cm/cm

@Temperature 80.0 - 80.0 °C
0.00900 - 0.00900 in/in

@Temperature 176 - 176 °F
Average value: 0.00900 cm/cm Grade Count:1
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Linear Mold Shrinkage, Transverse 0.00500 - 0.00900 cm/cm
0.00500 - 0.00900 in/in
Average value: 0.00770 cm/cm Grade Count:5
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..