Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00884 cm/cm Grade Count:13 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00252 cm/cm Grade Count:23 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.00118 cm/cm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.00119 cm/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00600 cm/cm | 0.000500 - 0.00600 in/in | Average value: 0.00180 cm/cm Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0140 cm/cm | 0.000500 - 0.0140 in/in | Average value: 0.00563 cm/cm Grade Count:669 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0250 cm/cm | 0.000500 - 0.0250 in/in | Average value: 0.00217 cm/cm Grade Count:18 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00488 cm/cm Grade Count:39 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00550 cm/cm | 0.000500 - 0.00550 in/in | Average value: 0.00210 cm/cm Grade Count:21 |
Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0120 cm/cm | 0.000500 - 0.0120 in/in | Average value: 0.00394 cm/cm Grade Count:76 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00700 cm/cm | 0.000500 - 0.00700 in/in | Average value: 0.00476 cm/cm Grade Count:16 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0250 cm/cm | 0.000500 - 0.0250 in/in | Average value: 0.0136 cm/cm Grade Count:218 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00800 cm/cm | 0.000500 - 0.00800 in/in | Average value: 0.00304 cm/cm Grade Count:14 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00600 cm/cm | 0.000500 - 0.00600 in/in | Average value: 0.00240 cm/cm Grade Count:29 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00700 cm/cm | 0.000500 - 0.00700 in/in | Average value: 0.00256 cm/cm Grade Count:44 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0140 cm/cm | 0.000500 - 0.0140 in/in | Average value: 0.00686 cm/cm Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00342 cm/cm Grade Count:26 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00466 cm/cm Grade Count:151 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0200 cm/cm | 0.000500 - 0.0200 in/in | Average value: 0.00262 cm/cm Grade Count:50 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0180 cm/cm | 0.000500 - 0.0180 in/in | Average value: 0.00327 cm/cm Grade Count:31 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00900 cm/cm | 0.000500 - 0.00900 in/in | Average value: 0.00262 cm/cm Grade Count:34 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00300 cm/cm | 0.000500 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00421 cm/cm Grade Count:132 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00800 cm/cm | 0.000500 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:101 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0100 cm/cm | 0.000500 - 0.0100 in/in | Average value: 0.00311 cm/cm Grade Count:14 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.100 cm/cm | 0.000500 - 0.100 in/in | Average value: 0.0248 cm/cm Grade Count:5 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00348 cm/cm Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0260 cm/cm | 0.000500 - 0.0260 in/in | Average value: 0.00646 cm/cm Grade Count:53 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |