Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.10 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.400 - 2.10 J/cm²
1.90 - 9.99 ft-lb/in²
Average value: 1.28 J/cm² Grade Count:12
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Charpy Impact, Notched 0.900 - 2.10 J/cm²
4.28 - 9.99 ft-lb/in²
Average value: 1.32 J/cm² Grade Count:14
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact, Notched 1.20 - 2.10 J/cm²
5.71 - 9.99 ft-lb/in²
Average value: 1.63 J/cm² Grade Count:6
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.300 - 2.10 J/cm²

@Temperature -40.0 - 30.0 °C
1.43 - 9.99 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 1.09 J/cm² Grade Count:46
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact, Notched 0.800 - 2.10 J/cm²

@Temperature -30.0 - 30.0 °C
3.81 - 9.99 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.22 J/cm² Grade Count:18
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact, Notched 0.700 - 2.10 J/cm²

@Temperature -40.0 - -30.0 °C
3.33 - 9.99 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.972 J/cm² Grade Count:7
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..