Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 - 2.10 J/cm² | 1.90 - 9.99 ft-lb/in² | Average value: 1.28 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact, Notched | 0.900 - 2.10 J/cm² | 4.28 - 9.99 ft-lb/in² | Average value: 1.32 J/cm² Grade Count:14 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 1.20 - 2.10 J/cm² | 5.71 - 9.99 ft-lb/in² | Average value: 1.63 J/cm² Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.300 - 2.10 J/cm² @Temperature -40.0 - 30.0 °C |
1.43 - 9.99 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 1.09 J/cm² Grade Count:46 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 0.800 - 2.10 J/cm² @Temperature -30.0 - 30.0 °C |
3.81 - 9.99 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.22 J/cm² Grade Count:18 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact, Notched | 0.700 - 2.10 J/cm² @Temperature -40.0 - -30.0 °C |
3.33 - 9.99 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.972 J/cm² Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |