Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 6.60 mm |
167 °F @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 6.60 mm |
167 °F @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
PTS PCA-3013 High Flow PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
PTS PCA-30G00 Impact Modified Polycarbonate/PBT Alloy For Cold Temperature Impact.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 75.0 - 130 °C | 167 - 266 °F | Average value: 112 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
UL RTI, Electrical | 75.0 - 140 °C | 167 - 284 °F | Average value: 114 °C Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
UL RTI, Electrical | 75.0 - 125 °C | 167 - 257 °F | Average value: 120 °C Grade Count:11 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **) Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.00 - 1.10 mm |
167 °F @Thickness 0.0394 - 0.0433 in |
|
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness >=1.50 mm |
167 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC (Asia Pacific) Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | UL 746B |
Covestro Makroblend® UT305 PC/PET Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• High moisture en.. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
Covestro Makrolon® 2205 Polycarbonate, Injection Grade Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc.. |
|||
UL RTI, Electrical | 75.0 °C | 167 °F | |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
UL RTI, Electrical | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
|
Covestro Makrolon® 1143 Polycarbonate Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate.. |