Mechanical Properties Metric English Comments
Modulus of Elasticity 6.60 - 13.8 GPa
957 - 2000 ksi
Average value: 11.5 GPa Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Modulus of Elasticity 2.80 - 13.8 GPa
406 - 2000 ksi
Average value: 7.28 GPa Grade Count:22
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Modulus of Elasticity 0.930 - 13.8 GPa
135 - 2000 ksi
Average value: 6.49 GPa Grade Count:74
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Modulus of Elasticity 2.41 - 13.8 GPa
350 - 2000 ksi
Average value: 6.03 GPa Grade Count:86
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Modulus of Elasticity 4.48 - 13.8 GPa
650 - 2000 ksi
Average value: 6.61 GPa Grade Count:24
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Modulus of Elasticity 11.0 - 13.8 GPa
1600 - 2000 ksi
Average value: 12.0 GPa Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..