Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm |
356 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE) Linen reinforcement, Phenolic resin, Tan / Black color. Good electrical and high mechanical strength. Moisture resistant.Information provided by Pyrotek. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Dielectric Strength | 14.0 - 35.0 kV/mm | 356 - 889 kV/in | Average value: 22.1 kV/mm Grade Count:49 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Dielectric Strength | 14.0 - 34.0 kV/mm | 356 - 864 kV/in | Average value: 23.3 kV/mm Grade Count:14 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
356 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
356 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.00 mm |
356 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Dielectric Strength | 14.0 - 111 kV/mm | 356 - 2820 kV/in | Average value: 50.0 kV/mm Grade Count:55 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 150°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 70°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Dielectric Strength | 14.0 kV/mm @Frequency 60.0 Hz |
356 kV/in @Frequency 60.0 Hz |
short time, wet; ASTM D149 |
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic RX 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America, Inc. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | IEC 60243-1 |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | IEC 60243-1 |
Polyplastics Duranex® 6302T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 2.8 kV minimum |
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 2.8 kV minimum |
Arlon 0.015" (0.381 mm) Primerless Thermabond® Uncured Silicone (99990A015) 0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038).. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.00 mm |
356 kV/in @Thickness 0.118 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.00 mm |
356 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.00 mm |
356 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 - 100 kV/mm | 356 - 2540 kV/in | Average value: 35.8 kV/mm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6 18% crystallinity. Information supplied by Elastomer Engineering. |