Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Average value: 5.00 J Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Average value: 5.00 J Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC STAMAX 30YK270 PP SABIC® STAMAX 30YK270 is a 30% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66 LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66 LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF0059 PA 66 LNP THERMOCOMP* RF0059 is a compound based on Nylon 66 resin containing 25% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific) LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Total energy; ASTM D3763 |
Styrolution Styrolux® GH 62 SBC Description: Styrolux® GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warp.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific) LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | ISO 6603-1 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | ASTM Test |
BASF Styroclear GH 62 SBC Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Dart Drop, Total Energy | 5.00 - 8.00 J | 3.69 - 5.90 ft-lb | Average value: 6.79 J Grade Count:14 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |