Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AH Acetal Homopolymer LNP* LUBRICOMP* KP004AH is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific) LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | ISO 6603-1 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | ASTM D3763 |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Dart Drop, Total Energy | 5.00 - 8.00 J | 3.69 - 5.90 ft-lb | Average value: 6.79 J Grade Count:14 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Dart Drop, Total Energy | <= 5.00 J | <= 3.69 ft-lb | ISO 6603-1 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |