Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
Reliance Industries Polypropylene - 40% Suzorex mica (surface treated) filled Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CM100LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding Medium impact, nucleated, antistat, injection molding. Applications: Household articles, pails, consumer products.Information provided by Phillips 66. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
Flint Hills AP5206-HN Polypropylene Impact Copolymer Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.Applications: Compression and injection molding: caps and closuresInformation Provided b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 3-9230 KAR BU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR BU is a black colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR BU is develope.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ISO 75-1/-2 |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ISO 75 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ISO 75 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C @Thickness 6.40 mm |
226 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | 0.125 inch; ASTM D648 |
PlastxWorld CEVIAN®-V 400T ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI 40% Talc Reinforced PP HomopolymerApplications: Sheets, Pipes, ProfilesProcessing: ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 227 °F | ASTM D648 |
ExxonMobil AXO3BE3 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
Covestro Texin® 4215 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
Cheng Yu Plastic A706G15 SAN, 15% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **) Injection molding grade, improved flow.Applications: Automotive industry: e.g. wheel trims, instrument panel components.Information provided by the manufacturer.Novodur is produced by Styrolution (2.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | |
Polimeri Europa KOBLEND PCA 53 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 110°C Main application fiel.. |