Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole

Category Polymer , Thermoplastic , Polybenzimidazole (PBI)
Manufacturer PBI Performance Products, Inc.
Trade Name Celazole®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. Celazole® T-Series products combine the superior mechanical properties and thermal resistance of PBI with the melt process ability of polyaryletherketones.Designed for injection molding and extrusionTF-60V is a glass-reinforced blend offering thermal and electrical insulation, wear resistance and dimensional stability with the cost efficiency of a direct form process. An excellent choice for high temperature electrical insulators, plasma torch drag cup shields, swirl baffles and parts requiring minimal thermal expansion.Information provided by PBI Performance Products
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
Water Absorption 0.25 %

@Temperature 22.8 °C,
Time 86400 sec
0.25 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 4.6 %
4.6 %
ASTM D570
Loss On Ignition 5.0 %

@Temperature 607 °C
5.0 %

@Temperature 1120 °F
Air; ASTM TGA
5.0 %

@Temperature 635 °C
5.0 %

@Temperature 1180 °F
Nitrogen; ASTM TGA
Mechanical Properties Metric English Comments
Hardness, Rockwell A 30
30
ASTM D785
Tensile Strength 150 MPa
21800 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
Tensile Modulus 12.0 GPa
1740 ksi
Flexural Strength 225 MPa
32600 psi
ASTM D790
Flexural Modulus 12.5 GPa
1810 ksi
Compressive Strength 220 MPa
31900 psi
ASTM D695
Compressive Modulus 3.60 GPa
522 ksi
Poissons Ratio 0.34
0.34
Shear Modulus 4.48 GPa
650 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 25.0 - 150 °C
9.44 µin/in-°F

@Temperature 77.0 - 302 °F
ASTM TMA
Specific Heat Capacity 1.13 J/g-°C

@Temperature 70.0 °C
0.270 BTU/lb-°F

@Temperature 158 °F
ASTM D648
Thermal Conductivity 0.360 W/m-K

@Temperature 23.9 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 75.0 °F
ASTM F-433
Deflection Temperature at 1.8 MPa (264 psi) 310 °C
590 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
ASTM D150
3.9

@Frequency 10000 Hz
3.9

@Frequency 10000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 10000 Hz
0.0010

@Frequency 10000 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495