Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 24.0 - 138 MPa | 3480 - 20000 psi | Average value: 40.4 MPa Grade Count:64 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Tensile Strength, Ultimate | 29.0 - 138 MPa | 4210 - 20000 psi | Average value: 72.7 MPa Grade Count:55 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Tensile Strength, Ultimate | 45.0 - 138 MPa | 6530 - 20000 psi | Average value: 93.7 MPa Grade Count:35 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Tensile Strength, Ultimate | 65.5 - 138 MPa | 9500 - 20000 psi | Average value: 95.2 MPa Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 68.9 - 138 MPa | 10000 - 20000 psi | Average value: 115 MPa Grade Count:15 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Tensile Strength, Ultimate | 9.28 - 138 MPa @Temperature -20.0 - 200 °C |
1350 - 20000 psi @Temperature -4.00 - 392 °F |
Average value: 49.7 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Tensile Strength, Ultimate | 9.28 - 138 MPa @Strain 0.230 - 4.21 % |
1350 - 20000 psi @Strain 0.230 - 4.21 % |
Average value: 49.7 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Tensile Strength, Ultimate | 34.0 - 138 MPa | 4930 - 20000 psi | Average value: 76.3 MPa Grade Count:61 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 82.7 - 138 MPa | 12000 - 20000 psi | Average value: 95.9 MPa Grade Count:6 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Ultimate | 48.3 - 138 MPa | 7000 - 20000 psi | Average value: 88.2 MPa Grade Count:45 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 86.2 - 138 MPa | 12500 - 20000 psi | Average value: 110 MPa Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |