Polymer Property : Izod Impact, Notched = 0.800 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 4008 T Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products G13P100-00UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Natural
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 4001 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Izod Impact, Notched 0.427 - 0.641 J/cm
0.800 - 1.20 ft-lb/in
Average value: 0.547 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 AF10 HS L Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Fric..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 AF10 Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionInformation provided by..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Techmer ES Plaslube® J-80/20/TF/15 BK223 Acetal (POM) Copolymer
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Techmer ES Plaslube® NY-1/MS/5 NAT PA66
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Formosa Plastics Formolene® 3335N Random Copolymer Polypropylene
Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3335N is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for thin walled, injec..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.20 mm
0.800 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company EMI 2161 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Izod Impact, Notched 0.427 J/cm

@Thickness 3.20 mm
0.800 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company EMI 261 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company ESD C 2500 Polycarbonate/ABS Alloy (PC/ABS), ESD Protection - Electrically Conductive
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company PermaStat® 601 FR Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - Flame Retardant - ESD Protection - Permanently Anti-static
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 0899 X 87096 EG BLACK Acetal (POM)
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 100 GB 10 Polypropylene (PP), Glass Bead
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 127 HF Polypropylene (PP), Talc - High Flow
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 199 X 102002 Polypropylene (PP), Glass Bubbles
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 200 A Nylon 6 (PA), Unreinforced - UL94 V-2 (NC) - UL94 HB (All Colors)
Izod Impact, Notched 0.427 J/cm

@Thickness 3.20 mm
0.800 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 2200 HF Polyetheretherketone (PEEK); High Flow
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company ESD A 1307 Polyphenylene Sulfide (PPS), Glass Fiber - ESD Protection - Static Dissipative
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 2388 Glass Reinforced Polypropylene
DescriptionPolyfort® FPP 2388 is a 5% glass reinforced polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256A
ExxonMobil Exxtral™ MDK340 Performance Polyolefin
Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Multibase Multi-Flam™ 0106 PP Polypropylene
Features:Flame RetardantHalogenated Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase
Izod Impact, Notched 0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® AT-25GF-10MN/000 BLASCK Acetal-Copolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 4783 Polytrimethylene Terephthalate (PTT), Carbon Fiber
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2100 TFE 15 Polyetherimide (PEI), PTFE Lubricated