Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
1.43 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL B63 HH Nylon 6 for injection molding Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Average value: 0.435 J/cm² Grade Count:10 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO Data |
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/1eA |
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® LS 87 HDPE Made for special applicationsInformation provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65 Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 30.0 °C |
1.43 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65 Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179 |
BASF Ultramid® 8202 HS BK-102 PA6 (Dry) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
BASF Novolen® 1102 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.300 - 8.50 J/cm² | 1.43 - 40.5 ft-lb/in² | Average value: 1.41 J/cm² Grade Count:9 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.300 - 4.50 J/cm² | 1.43 - 21.4 ft-lb/in² | Average value: 2.14 J/cm² Grade Count:42 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |