Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 24.1 - 207 MPa | 3500 - 30000 psi | Average value: 150 MPa Grade Count:55 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Yield Strength | 85.0 - 207 MPa | 12300 - 30000 psi | Average value: 151 MPa Grade Count:37 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Flexural Yield Strength | 93.1 - 207 MPa | 13500 - 30000 psi | Average value: 142 MPa Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 10.0 - 207 MPa | 1450 - 30000 psi | Average value: 52.0 MPa Grade Count:48 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Flexural Yield Strength | 25.0 - 207 MPa @Temperature -40.0 - 120 °C |
3630 - 30000 psi @Temperature -40.0 - 248 °F |
Average value: 84.2 MPa Grade Count:6 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 58.6 - 207 MPa | 8500 - 30000 psi | Average value: 130 MPa Grade Count:89 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 75.8 - 207 MPa | 11000 - 30000 psi | Average value: 130 MPa Grade Count:47 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 128 - 207 MPa | 18500 - 30000 psi | Average value: 169 MPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Flexural Yield Strength | 103 - 207 MPa | 15000 - 30000 psi | Average value: 153 MPa Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Flexural Yield Strength | 83.0 - 207 MPa | 12000 - 30000 psi | Average value: 158 MPa Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Flexural Yield Strength | 77.9 - 207 MPa | 11300 - 30000 psi | Average value: 109 MPa Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |