Polymer Property : Izod Impact, Unnotched (ISO) = 80.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 30.0 - 80.0 kJ/m²
14.3 - 38.1 ft-lb/in²
Average value: 52.4 kJ/m² Grade Count:45
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Izod Impact, Unnotched (ISO) 33.0 - 80.0 kJ/m²
15.7 - 38.1 ft-lb/in²
Average value: 52.0 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Izod Impact, Unnotched (ISO) 27.0 - 80.0 kJ/m²

@Temperature -30.0 - -30.0 °C
12.8 - 38.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 46.8 kJ/m² Grade Count:5
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Unnotched (ISO) 15.0 - 80.0 kJ/m²
7.14 - 38.1 ft-lb/in²
Average value: 34.0 kJ/m² Grade Count:18
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Unnotched (ISO) 76.0 - 80.0 kJ/m²

@Temperature -30.0 - -30.0 °C
36.2 - 38.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 78.0 kJ/m² Grade Count:2
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Izod Impact, Unnotched (ISO) 10.0 - 80.0 kJ/m²
4.76 - 38.1 ft-lb/in²
Average value: 34.7 kJ/m² Grade Count:9
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Unnotched (ISO) 11.0 - 80.0 kJ/m²
5.23 - 38.1 ft-lb/in²
Average value: 31.5 kJ/m² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..