Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | DIN 52612 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | DIN 52612 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | DIN 52612 |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East) LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 650 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1200 °F |
ASTM C177 |
Unifrax IsoMat® AV/AVi Substrate Support Mat Developed to meet the most stringent European regulatory requirements, IsoMat AV/Avi is engineered utilizing the unique Isofrax® 1260°C fibers - a revolutionary green fiber produced using patented.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 650 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1200 °F |
ASTM C177 |
Unifrax IsoMat® AV5 Substrate Support Mat IsoMat AV5 is designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.IsoMat AV5 offers superior performance at low tem.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 650 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1200 °F |
ASTM C177 |
Unifrax XPE® NV Substrate Support Mat XPE® intumescent mat products are designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.Unifrax offers a variety of .. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® 4000 Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist .. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 45.0 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 113 °F |
|
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 45.0 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 113 °F |
|
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 45.0 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 113 °F |
|
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | ASTM E1530 |
3M Scotchcast™ 265 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 600 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Pyrotek Wollite 45 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® LD 500 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Thermal Conductivity | 0.180 W/m-K | 1.25 BTU-in/hr-ft²-°F | |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |