Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 90.0 sec Grade Count:6 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Hot Wire Ignition, HWI | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 90.0 sec Grade Count:5 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Hot Wire Ignition, HWI | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 108 sec Grade Count:5 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Hot Wire Ignition, HWI | 60.0 - 150 sec | 60.0 - 150 sec | Average value: 120 sec Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |