Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 - 5.50 J/cm² | 9.52 - 26.2 ft-lb/in² | Average value: 3.82 J/cm² Grade Count:14 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact Unnotched | 2.60 - 5.50 J/cm² | 12.4 - 26.2 ft-lb/in² | Average value: 3.77 J/cm² Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Charpy Impact Unnotched | 1.50 - 5.50 J/cm² | 7.14 - 26.2 ft-lb/in² | Average value: 3.75 J/cm² Grade Count:4 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 5.50 - 5.50 J/cm² @Temperature -30.0 - -30.0 °C |
26.2 - 26.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.50 J/cm² Grade Count:1 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 2.50 - 5.50 J/cm² | 11.9 - 26.2 ft-lb/in² | Average value: 4.17 J/cm² Grade Count:3 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact Unnotched | 2.70 - 5.50 J/cm² | 12.8 - 26.2 ft-lb/in² | Average value: 4.17 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 2.20 - 5.50 J/cm² @Temperature -30.0 - -30.0 °C |
10.5 - 26.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.64 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 1.30 - 5.50 J/cm² | 6.19 - 26.2 ft-lb/in² | Average value: 3.10 J/cm² Grade Count:19 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact Unnotched | 2.00 - 5.50 J/cm² @Temperature -30.0 - -20.0 °C |
9.52 - 26.2 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.12 J/cm² Grade Count:18 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact Unnotched | 3.00 - 5.50 J/cm² | 14.3 - 26.2 ft-lb/in² | Average value: 4.40 J/cm² Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Charpy Impact Unnotched | 2.00 - 5.50 J/cm² | 9.52 - 26.2 ft-lb/in² | Average value: 3.92 J/cm² Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |