Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.427 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment
Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Omni Plastics OmniTuff™ HPP CCF40 Homopolymer Polypropylene Calcium Carbonate Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256 Type A
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Izod Impact, Notched 0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ AT-15GM/15T Acetal-Copolymer, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.427 J/cm

@Diameter 0.125 mm,
Temperature -20.0 °C
0.800 ft-lb/in

@Diameter 0.00492 in,
Temperature -4.00 °F
bar; ASTM D256
Ineos L12Z-01 Polypropylene Impact Copolymer
Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provi..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers PPH-110 Polypropylene, Homopolymer
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® ABS CF10 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PA6/6 C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 CM25 HS BK 25% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 TS15 BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, ..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Techmer ES Plaslube® J-80/20/TF/15 NAT Acetal (POM) Copolymer
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Washington Penn Medium Impact Copolymer 40% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Formosa Plastics Formolene® 1103K Homopolymer Polypropylene
Homopolymer for BOPP Film Formolene® 1103K is a high molecular weight, highly isotactic, polypropylene homopolymer designed for extrusion processes notably slit tape applications. It contains a uni..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 102 FR Polypropylene (PP), Glass Fiber - Flame Retardant
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 200 A Nylon 6 (PA), Unreinforced - UL94 V-2 (NC) - UL94 HB (All Colors)
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2187 HEC Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 281 MS Nylon 6/6 (PA), Carbon Fiber - Molybdenum Disulfide
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 281 TFE 15 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 200 D AR 10 TFE 5 Nylon 6/12 (PA), Aramid Fiber - PTFE Lubricated
Izod Impact, Notched 0.427 J/cm

@Temperature 22.8 °C
0.800 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber
Data provided by Clariant Masterbatches
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336G5M25CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.427 J/cm

@Thickness 3.18 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 200B AR 10 TFE 10  Nylon 6/10 (PA 6/10) Aramid Fiber 10% - PTFE 10%  (discon
Aramid Fiber 10% - PTFE 10%Comments:Aramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256 Type A
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet)
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 200 A GB 25 Nylon 6 (PA), Glass Bead
Copyright © lookpolymers.com All Rights Reserved