Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 27.0 - 80.0 kJ/m² @Temperature -30.0 - -30.0 °C |
12.8 - 38.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 46.8 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL139P PC LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12 LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66 LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66 LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 27.0 kJ/m² | 12.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |