Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 1.00 - 7.00 J | 0.738 - 5.16 ft-lb | Average value: 4.50 J Grade Count:8 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Dart Drop, Total Energy | 3.00 - 7.00 J @Temperature -30.0 - -20.0 °C |
2.21 - 5.16 ft-lb @Temperature -22.0 - -4.00 °F |
Average value: 3.75 J Grade Count:3 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |