Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 30%Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.46 - 1.70 g/cc
0.0527 - 0.0614 lb/in³
Average value: 1.60 g/cc Grade Count:22
Filler Content 25.0 - 30.0 %
25.0 - 30.0 %
Average value: 29.6 % Grade Count:12
Water Absorption 0.300 - 1.60 %
0.300 - 1.60 %
Average value: 0.440 % Grade Count:15
Additive Loading 30.0 %
30.0 %
Average value: 30.0 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00232 cm/cm Grade Count:21
Linear Mold Shrinkage, Transverse 0.00580 - 0.00800 cm/cm
0.00580 - 0.00800 in/in
Average value: 0.00660 cm/cm Grade Count:3
Melt Flow 4.50 - 25.0 g/10 min
4.50 - 25.0 g/10 min
Average value: 10.6 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120 - 123
120 - 123
Average value: 123 Grade Count:7
Tensile Strength, Ultimate 50.0 - 150 MPa
7250 - 21800 psi
Average value: 125 MPa Grade Count:18
10.0 - 135 MPa

@Temperature 60.0 - 150 °C
1450 - 19600 psi

@Temperature 140 - 302 °F
Average value: 70.2 MPa Grade Count:2
31.0 - 43.0 MPa

@Temperature 180 - 180 °C
4500 - 6240 psi

@Temperature 356 - 356 °F
Average value: 70.2 MPa Grade Count:1
31.0 - 43.0 MPa

@# of Cycles 100000 - 1.00e+7
4500 - 6240 psi

@# of Cycles 100000 - 1.00e+7
Average value: 70.2 MPa Grade Count:1
50.0 - 80.0 MPa

@Temperature 160 - 160 °C
7250 - 11600 psi

@Temperature 320 - 320 °F
Average value: 70.2 MPa Grade Count:1
50.0 - 80.0 MPa

@Strain 0.600 - 1.40 %
7250 - 11600 psi

@Strain 0.600 - 1.40 %
Average value: 70.2 MPa Grade Count:1
Tensile Strength, Yield 125 - 169 MPa
18200 - 24500 psi
Average value: 142 MPa Grade Count:5
Elongation at Break 1.40 - 4.00 %
1.40 - 4.00 %
Average value: 2.37 % Grade Count:21
2.10 - 2.50 %

@Temperature 60.0 - 150 °C
2.10 - 2.50 %

@Temperature 140 - 302 °F
Average value: 2.33 % Grade Count:1
Modulus of Elasticity 6.60 - 10.9 GPa
957 - 1580 ksi
Average value: 9.31 GPa Grade Count:20
8.60 - 10.0 GPa

@Temperature 60.0 - 160 °C
1250 - 1450 ksi

@Temperature 140 - 320 °F
Average value: 9.41 GPa Grade Count:2
Flexural Yield Strength 172 - 221 MPa
25000 - 32100 psi
Average value: 192 MPa Grade Count:19
Flexural Modulus 7.58 - 11.3 GPa
1100 - 1640 ksi
Average value: 8.54 GPa Grade Count:19
Compressive Yield Strength 124 - 145 MPa
18000 - 21000 psi
Average value: 140 MPa Grade Count:5
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Izod Impact, Notched 0.641 - 1.07 J/cm
1.20 - 2.00 ft-lb/in
Average value: 0.822 J/cm Grade Count:18
Izod Impact, Unnotched 3.74 - 7.47 J/cm
7.00 - 14.0 ft-lb/in
Average value: 5.91 J/cm Grade Count:13
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 42.0 - 59.0 kJ/m²

@Temperature -25.0 - 120 °C
20.0 - 28.1 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 52.7 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 - 4.20 J/cm²
11.9 - 20.0 ft-lb/in²
Average value: 3.40 J/cm² Grade Count:3
4.50 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
Average value: 0.733 J/cm² Grade Count:3
0.800 - 0.800 J/cm²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.800 J/cm² Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 15.0 - 36.0 µm/m-°C
8.33 - 20.0 µin/in-°F
Average value: 28.2 µm/m-°C Grade Count:12
17.0 - 17.0 µm/m-°C

@Temperature 140 - 180 °C
9.44 - 9.44 µin/in-°F

@Temperature 284 - 356 °F
Average value: 17.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.230 - 0.317 W/m-K
1.60 - 2.20 BTU-in/hr-ft²-°F
Average value: 0.295 W/m-K Grade Count:4
Maximum Service Temperature, Air 185 - 220 °C
365 - 428 °F
Average value: 203 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 215 - 222 °C
419 - 432 °F
Average value: 219 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 204 - 220 °C
400 - 428 °F
Average value: 214 °C Grade Count:22
Glass Transition Temp, Tg 225 °C
437 °F
Average value: 225 °C Grade Count:3
Flammability, UL94 V-0
V-0
Grade Count:18
Oxygen Index 40.0 - 44.5 %
40.0 - 44.5 %
Average value: 42.2 % Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 2.00e+16 ohm-cm
1.00e+12 - 2.00e+16 ohm-cm
Average value: 8.00e+15 ohm-cm Grade Count:15
Surface Resistance 1.00e+14 - 1.00e+15 ohm
1.00e+14 - 1.00e+15 ohm
Average value: 4.00e+14 ohm Grade Count:3
Dielectric Constant 4.11 - 4.30
4.11 - 4.30
Average value: 4.18 Grade Count:8
Dielectric Strength 14.6 - 37.0 kV/mm
370 - 940 kV/in
Average value: 18.4 kV/mm Grade Count:11
Dissipation Factor 0.00180 - 0.0100
0.00180 - 0.0100
Average value: 0.00529 Grade Count:8
Arc Resistance 75.0 - 120 sec
75.0 - 120 sec
Average value: 84.0 sec Grade Count:5
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Average value: 354 °C Grade Count:6
Melt Temperature 343 - 399 °C
649 - 750 °F
Average value: 365 °C Grade Count:12
Mold Temperature 135 - 190 °C
275 - 374 °F
Average value: 157 °C Grade Count:17
Drying Temperature 149 - 180 °C
300 - 356 °F
Average value: 156 °C Grade Count:10
Moisture Content 0.0400 %
0.0400 %
Average value: 0.0400 % Grade Count:5
Dew Point -31.7 °C
-25.0 °F
Average value: -31.7 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:11
Users viewing this material also viewed the following: