Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
PolyOne Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-30GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific) 30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) 30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® ABS E GM30 LE 30% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0029EC PC LNP* STAT-KON* DE0029EC is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3710 is a 45% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 7.58 - 13.1 GPa | 1100 - 1900 ksi | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
PolyOne Nymax™ GF 1800 33 BLACK 13 Nylon 612 with 33% Glass Fiber
(discontinued **) Molded Test Bars: Dry as Molded |
|||
Flexural Modulus | 7.58 - 28.3 GPa | 1100 - 4100 ksi | Average value: 17.0 GPa Grade Count:32 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |