Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638-95 |
Multibase Multi-Pro® 0112 Black Polypropylene Multi-Pro 0112 is a nucleated and antistated polypropylene homopolymer. It is designed for injection molding applications that require superior mold release properties.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638-61T |
Rotuba 860MS 686.5 Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM Data |
Americas Styrenics Styron® 495R High Impact Polystyrene
(discontinued **) Data provided by Dow Chemical.Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formatio.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated
(discontinued **) Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Tensile Strength, Ultimate | 31.0 - 42.1 MPa | 4500 - 6100 psi | Average value: 36.9 MPa Grade Count:7 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Ultimate | 31.0 - 210 MPa | 4500 - 30500 psi | Average value: 161 MPa Grade Count:23 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Tensile Strength, Ultimate | 31.0 MPa @Temperature 22.0 °C |
4500 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Tensile Strength, Ultimate | 31.0 MPa @Temperature 22.0 °C |
4500 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | 2 in/min; ASTM D638 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | 2 in/min.; ASTM D638 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Tensile Strength, Ultimate | 31.0 MPa @Temperature 22.0 °C |
4500 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM Data |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM Data |
Styron Magnum™ 9035 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM Data |
Styron Magnum™ 9555 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D412 |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ISO 527-1/-2 |
DSM Arnitel® EM631-HB TPC-ET Extrusion Grade, Heat Stabilized |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638-95 |
Multibase Multi-ABS 3522 Utility Grade Multi-ABS 3522 utility grade is a black ABS resin produced for wide-specs and recycled resins. This product is suitable for automotive application and for non-critical load bearing parts.Data provid.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | XY; ASTM D638 |
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued ** Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed.. |
|||
Tensile Strength, Ultimate | 31.0 MPa | 4500 psi | ASTM D638 |
Petromont 7002 Medium Density Polyethylene Resin Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |