Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 225 °C | 437 °F | D3482 |
Ovation Polymers UTTAP SF 50030GF Polyethersulfone, 30% Glass Reinforced Glass reinforced (30 %) Polyether Sulfone, excellent chemical and electrical resistance, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50%.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber Excellent chemical and electrical resistance, high stiffness, modulus and HDTAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
Cookson Group Plaskon® SMT-B-1LV Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). Using an improved optimized filler system, it provide.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5111 PEI 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5211R PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific) 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3418 |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | Average value: 225 °C Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | Average value: 225 °C Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | DSC |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |