Polymer Property : Injection Pressure = 103 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 302 SI 2 FR Polycarbonate (PC), Glass Fiber - Silicone Lubricated - Flame Retardant
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 383 TFE 10 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 400 Polystyrene (PS), General Purpose
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 4700 TFE 18 SI 2  Polytrimethylene Terephthalate (PTT) PTFE 18% - Silicone 2% &nb
PTFE 18% - Silicone 2%Comments:PTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pro..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 800 TFE 10 SI 2 DEL Acetal (POM), PTFE Lubricated - Silicone Lubricated - Homopolymer
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP PP 40 GF NAT Polypropylene (PP); Value Product - Glass Fiber - Chemically Coupled
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 211G HS  Nylon 4/6 (PA 4/6) Glass Fiber 60% - Heat Stable  (discontinued **)
Glass Fiber 60% - Heat StableComments:Glass FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Infor..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company PermaStat® 200F  Nylon 12 (PA 12) Anti-Static  (discontinued **)
Anti-StaticComments:Permanently Anti-StaticESD ProtectionUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 102 CC HI Polypropylene (PP), Glass Fiber - High Impact - Chemically Coupled
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 105 Polypropylene (PP), Glass Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1387 TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1399 X 130032 A Polyphenylene Sulfide (PPS); Thermally Conductive - Glass Fiber - Electrically Conductive - EMI/RFI Shielding - (Preliminary Data Sheet)
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 199 X 125445 B Polypropylene (PP), Cellulose Fiber - 30% Renewable Resource Content - Additional 56% Post Consumer Recycled Content
30% renewable content based on % of total compound weight.
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 2000 B-340 Polysulfone Alloy, Glass Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 2599 X 125737 C Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company ESD A 600 Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Static Dissipative
Injection Pressure 55.2 - 103 MPa
8000 - 15000 psi
RTP Company RTP 2099 X 124790 C Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 78% Renewable Resource Content
Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.
Injection Pressure 33.1 - 103 MPa
4800 - 15000 psi
Average value: 71.2 MPa Grade Count:20
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1400 AR 15  Polyethersulfone (PES) Aramid Fiber 15%  (discontinued **)
Aramid Fiber 15%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 300 TC-I-15 Polycarbonate (PC); Thermally Conductive - Electrically Insulative
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 4005.3 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 800.5 Acetal (POM), Glass Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 2740U-70A  Saturated Styrenic Elastomer (SBS) 70 Shore A  (discontinued **)&
70 Shore AComments:70-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Injection Pressure 2.76 - 103 MPa
400 - 15000 psi
Average value: 59.6 MPa Grade Count:9
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company PermaStat® 200 A Nylon 6 (PA), ESD Protection - Permanently Anti-static
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1201 S-90A Ester-based Thermoplastic Polyurethane Elastomer, Glass Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 207 A TFE 15 Nylon 6 (PA), Glass Fiber - PTFE Lubricated
Injection Pressure 55.2 - 103 MPa
8000 - 15000 psi
RTP Company RTP 2099 X 124789 A Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 94% Renewable Resource Content
Not optically transparent.  Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website.