Polymer Property : Shear Modulus = 29.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.200 GPa
29.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 0.200 GPa
29.0 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Modulus 0.200 GPa
29.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Modulus 0.200 GPa
29.0 ksi
torsional
DSM Fibre Intermediates Nyrim® 4000 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..
Shear Modulus 0.200 GPa
29.0 ksi
Cymat A35620SC 020SS Stabilized Aluminum Foam
Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it ..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:7
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Shear Modulus 0.200 - 1.00 GPa

@Temperature 50.0 - 225 °C
29.0 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..