Processing Properties Metric English Comments
Injection Pressure 68.9 - 82.7 MPa
10000 - 12000 psi
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 301 SI 2 Z Polycarbonate (PC), Glass Fiber - Silicone Lubricated - FDA Compliant Ingredients
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1385 HM  Polyphenylene Sulfide (PPS) Carbon Fiber 30% - High Modulus  (disco
Carbon Fiber 30% - High ModulusComments:Carbon FiberHigh ModulusUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 382 HEC FR Polycarbonate (PC) Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection - Flame Retardant
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 399 X 129955 U Polycarbonate (PC), Flame Retardant - Transparent - UV Stabilized
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 399 X 130942 A Polycarbonate (PC), Carbon Nanotube - High Purity - ESD Protection
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 4008 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 4083 Polyphthalamide (PPA); Carbon Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 600 GB 30 Acrylonitrile Butadiene Styrene (ABS), Glass Bead
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 603 TFE 13 SI 2 Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - PTFE Lubricated - Silicone Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 285D TFE 10  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 10%  (discontinued
Carbon Fiber 30% - PTFE 10%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company ESD 187 HF Polypropylene (PP) Carbon Fiber - High Flow - Electrically Conductive
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 199 X 125445 A Polypropylene (PP), Cellulose Fiber - 20% Renewable Resource Content - Additional 67% Post Consumer Recycled Content
20% renewable content based on % of total compound weight.
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 285 TFE 15 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 300 HF L UV Polycarbonate (PC), High Flow - Lubricated - UV Stabilized
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200 TFE 30 Nylon 6/6 (PA), PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 200 TFE 5 HS Nylon 6/6 (PA), PTFE Lubricated - Heat Stabilized
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 205 HS MS 5 Nylon 6/6 (PA), Glass Fiber - Molybdenum Disulfide - Heat Stabilized
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 207 A TFE 5 Nylon 6 (PA), Glass Fiber - PTFE Lubricated
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 205G TFE 15 HS  Nylon 4/6 (PA 4/6) Glass Fiber 30% - PTFE 15% - Heat Stable  
Glass Fiber 30% - PTFE 15% - Heat StableComments:Glass FiberPTFE LubricatedHeat Stabilized(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigmen..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 900 TFE 20  Polysulfone (PSU) PTFE 20%  (discontinued **)
PTFE 20%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for thi..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 1389 HEC  Polyphenylene Sulfide (PPS) Nickel-Coated Carbon Fiber 50% - EMI/ESD &n
Nickel-Coated Carbon Fiber 50% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 4005A TFE 15 SI 2  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 30% - PTFE 15% - Silicone 2%
Glass Fiber 30% - PTFE 15% - Silicone 2%Comments:Glass FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affe..
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 201 D SI 2 Nylon 6/12 (PA), Glass Fiber - Silicone Lubricated
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 2500 A TFE 15 Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
RTP Company RTP 283 Nylon 6/6 (PA); Carbon Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 883 Acetal (POM), Carbon Fiber
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company PermaStat® 200 H Impact-Modified Nylon 6/6 (PA), ESD Protection - Permanently Anti-static
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 3000 Polymethylpentene (PMP), Base Resin
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
RTP Company RTP 381 EM Polycarbonate (PC), Carbon Fiber - Easy Molding - Self Extinguishing - Halogen Free - UL94 V-2