Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistance = 1.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
STN 34 6460
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Radici Radiflam® S RV300AE (cond.) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Radici Radilon® S RV250 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Surface Resistance 1.00e+14 - 1.00e+15 ohm
1.00e+14 - 1.00e+15 ohm
IEC 60093
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Surface Resistance 1.00e+14 - 1.00e+15 ohm
1.00e+14 - 1.00e+15 ohm
IEC 60093
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Celanese FORTRON CES50 PPS, 40% Specialty  (Unverified Data**)
Fortron CES50 is a 40% glass fiber reinforced material with a total chlorine content less than or equal to 900 ppm. It offers excellent physical properties similar to those of the Fortron 1140L6 pr..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Evonik Corporation Vestodur® X4398 nf PBT  (discontinued **)
ISO data as provided by the manufacturer, Creanova, Inc.Low-temperature high impact PBT resin. For processing by injection molding and extrusion.This former Creanova product line is a part of Degus..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Celanese Hostaform® C 52021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with extremely high flowInformation provided by Celanese
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Styrolution Polystyrol 158 K GR 2 PS
Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned)
Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Techmer ES HiFill FR® PP CO FR HS
Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 93
Supreme Petrochem SP 6450 High Heat Polystyrene
Characteristics High impact and modulus Very good flow properties High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automo..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant
Flame retardant PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Covestro Bayblend® T 84 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Evonik Corporation Vestyron® 224 Polystyrene
Uses: Packaging made from thermoforming sheets blended with high impact polystyrene panels.ISO data as provided by the manufacturer.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257, IEC 93
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber
Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural
Information provided by Eurotec®
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural
Information provided by Eurotec®
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned)
Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Addiplast Addilene H 210 G20 Polypropylene Homopolymer
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
BASF Novolen® 2340 P Polypropylene
Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
BASF Ultradur S 4090 G6 30% Glass Filled PBT
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati..
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
DSM Akulon® K225-KS (Cond.) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Addiplast Addilene H 442 M30 Polypropylene Homopolymer
High heat resistance, detergent stabilizedInformation provided by Addiplast.
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
CENTROPLAST CENTROLYTE Polyethylene terephthalate
This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote..
Copyright © lookpolymers.com All Rights Reserved