Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.86 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 H-SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East)
Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability.
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Celanese Thermx® CG933 PCT, 30% Glass Reinforced  (Unverified Data**)
Thermx® CG933 is a 30% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.30% glass reinforced, flame retardantInformation provided by Celan..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Celanese Celcon® M140-L1 POM, Tribological  (Unverified Data**)
Celcon® M140-L1 is a general purpose acetal copolymer material with a slightly lower viscosity for improved flow in molding that has been modified to reduce or eliminate noise (squeak) when wearing..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East)
LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Celanese VECTRA E440i LCP, 42% Mineral / Glass Reinforced  (Unverified Data**)
Mineral and glass filled grade with low warp, easy flow and smooth surface apperance.Information provided by Celanese
Charpy Impact, Notched 0.600 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
2.86 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.58 J/cm² Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179
Total PPH 4022 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 4022 is a clarified nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4022 has been developed for extrusion-thermoforming, providing improved rigidity and impact r..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified
Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen ..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30
Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179-1eA
Barlog Plastics KEBAFORM C 270.0 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179-1eA
Barlog Plastics KEBAFORM C 901 VT POM Copolymer unreinforced, antistatic
POMInformation provided by BARLOG plastics GmbH.
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese Hostaform® C 9021 S1 POM, Tribological
Information provided by Celanese
Charpy Impact, Notched 0.600 J/cm²

@Thickness 4.00 mm,
Temperature 23.0 °C
2.86 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
Celanese Hostaform® C9021 M Acetal Copolymer with Molybdenum Disulphide
Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advant..
Charpy Impact, Notched 0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
ISO 179/1eA
Celanese Hostaform® S 27242 XAP2 ™ POM, Impact Modified
Easy flow, impact modified injection molding grade, with good low temperature impact strength and good weld line strength and reduced emissions. Emission according to VDA 275 < 5 mg/kgInformation pr..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2002AP Unreinforced Polybutylene Terephthalate
Description: Celanex 2002AP is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV and heat resistance. Celanex 2002AP is a..
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese Hostaform® C 13031 LS POM, UV Resistant
POM copolymerInformation provided by Celanese
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Celanese FORTRON 6450A6 PPS, 51% Specialty  (Unverified Data**)
Fortron 6450A6 is a fiberglass reinforced, mineral filled alloy that exhibits improved wear and sliding properties versus standard Fortron compounds.Low wear and lowest coefficient of frictionInform..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Celanese Hostaform® MT12U01 POM, Medical Technology
Hostaform« MT12U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12U01 is a moderately high flow grade for fa..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..
Copyright © lookpolymers.com All Rights Reserved