Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.86 - 11.3 GPa | 270 - 1640 ksi | Average value: 6.66 GPa Grade Count:99 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Flexural Modulus | 7.58 - 11.3 GPa | 1100 - 1640 ksi | Average value: 8.54 GPa Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |