Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 185 °C | 365 °F | Intermittent |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | Continuous |
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resist.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | short term |
Polikim KESTAMID® HS Polyamide 6, Heat Resistant Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with .. |
|||
Maximum Service Temperature, Air | 185 - 220 °C | 365 - 428 °F | Average value: 203 °C Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | Continuous use |
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | Continuous use |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Maximum Service Temperature, Air | 185 °C | 365 °F | |
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |