Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 381 TFE 10 SI 2 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 400 HI FR Polystyrene (PS), High Impact - Flame Retardant |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 400 HI Polystyrene (PS), High Impact |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 4009 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 600.5 HB Acrylonitrile Butadiene Styrene (ABS) Glass Fiber |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 701 SI 2 High Density Polyethylene (HDPE), Glass Fiber - Silicone Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | Average value: 86.2 MPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Injection Pressure | 4.96 - 103 MPa | 720 - 15000 psi | Average value: 81.3 MPa Grade Count:31 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 285G HS Nylon 4/6 (PA 4/6) Carbon Fiber 30% - Heat Stable
(discontinued ** Carbon Fiber 30% - Heat StableComments:Carbon FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Inf.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company EMI 660.6 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company ESD C 1080 TFE 15 Polybutylene Terephthalate (PBT), Carbon Fiber - Electrically Conductive - ESD Protection - PTFE Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company PermaStat® 600 Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 100 FR UV Polypropylene (PP) Flame Retardant - Non-PBDE/PBB |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 1005 TFE 5 Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 103 White Polypropylene (PP), Glass Fiber - NSF® RTP 103 White is certified under NSF® International Standard 14, compliant with Standard 61. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 103 Z Polypropylene (PP), Glass Fiber - FDA Compliant Ingredients |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 1004 FR A Polybutylene Terephthalate (PBT), Glass Fiber - Flame Retardant - UL94 V-0 RTP 1001 - 1005 FRA are a series of glass fiber reinforced, flame retardant PBT compounds. All are UL94 V-0 certified down to the 1/32" (0.8mm) thickness. These materials exhibit easy flow, excellen.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 1300 TFE 15 Polyphenylene Sulfide (PPS), PTFE Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | Average value: 86.2 MPa Grade Count:31 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 2700 S-70A FR Saturated Styrenic Block Copolymer, Flame Retardant - Non-PBDE/PBB
(discontinue Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 1389 HM Polyphenylene Sulfide (PPS) Carbon Fiber 50% - High Modulus
(disco Carbon Fiber 50% - High ModulusComments:Carbon FiberHigh ModulusUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | Average value: 86.2 MPa Grade Count:16 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 1405 B Polyethersulfone (PES) Glass Fiber 30%
(discontinued **) Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 299 A X 108950 I Nylon 6 (PA), High Gravity Compound |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 882 Acetal (POM), Carbon Fiber |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP 882 TFE 10 Acetal (POM), Carbon Fiber Reinforced - PTFE Lubricated |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company RTP PP FR2 Polypropylene (PP); Value Product - Flame Retardant |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
RTP Company ESD C 1200-80A Polyurethane Elastomer (TPU) Conductive - 80 Shore A
(discontin Conductive - 80 Shore AComments:ConductiveESD Protection80-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio.. |
|||
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | Average value: 86.2 MPa Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |