Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 80.0 sec Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Arc Resistance | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 6 (60-120 sec) |
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Arc Resistance | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 81.9 sec Grade Count:5 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | UL Rating PLC 6 (60-120 sec) |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL SE100P PPE+HIPS (Asia Pacific) |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp Noryl_SPN422L is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2110R PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 357U PBT+PC Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |